ASTM B296-96

Historical Standard: Standard Practice for Temper Designations of Magnesium Alloys, Cast and Wrought

ASTM B296

Scope

1.1 This practice covers a system for designating the tempers of magnesium alloys, cast and wrought. The designations used in ASTM specifications under the jurisdiction of Committee B-7 for magnesium alloy castings and wrought products, conform to this practice.

Keywords

Classification (standards); emmetals; Designation systems; Magnesium alloys; Temper; temper designations of magnesium alloys (cast/wrought), practice

ICS Code

ICS Number Code 77.120.20 (Magnesium and magnesium alloys)